Silver soldering 3/4 inch pipe with MAPP gas
I've read most of the threads on silver soldering and some suggest that it is possible to silver solder 3/4 inch pipe, but I'm still having problems getting enough heat into the fitting for the solder to flow. I'm attempting to join two 6m lengths of 3/4 inch type B copper pipe with a 8000 TS (from memory) MAPP gas torch. One of the pipes is mostly buried in the ground.
I can successfully join 1/2 inch pipe and I was wondering what I can do to get more heat into the joint?
-
2nd July 2007, 05:50 PM #2
G'day,
Probably pushing the BTU limits, but maybe a bit of excavation around the buried pipe and some heat sinks around the area.....like fire bricks or similar. I know from experience that house bricks go bang when they get hot enough.
Lots of cleaning/good flux, and good luck
-
2nd July 2007, 06:25 PM #3Member
- Join Date
- Dec 2006
- Location
- Canberra
- Age
- 45
- Posts
- 93
-
2nd July 2007, 06:28 PM #4
It can be done. I have just replace my hot water system. (this is what stopped me going to the woodworking show as it took all my spare cash )
I had to silver soldier one of the joints as it kept on leaking with soft soldier. I bought MAP just for the job and got it red hot and the silver soldier went straight on, with flux of course. Your problem maybe water in the pipe, if you can eliminate this you shouldn't have a problem.
Squirrel.
-
2nd July 2007, 09:12 PM #5Awaiting Email Confirmation
- Join Date
- Feb 2007
- Location
- Sydney
- Posts
- 87
Maybe I have the torch too close since the tip of the flame is nearly two inches from the nozzle. There was a little condensation in the buried pipe but it hasn't been used only buried.
Would a heat shield attachment make the difference?
Watson...Where can I get the fire bricks? I presume these are bricks for kilns and fireplaces.
-
3rd July 2007, 08:26 AM #6
I reckon you can get firebricks at one of those Coonara places.
-
3rd July 2007, 05:22 PM #7Member
- Join Date
- Dec 2006
- Location
- Canberra
- Age
- 45
- Posts
- 93
A bit of fibre cement sheeting can be very useful as a heat shield.
No need for flux if joining clean copper but you need it if joining to brass etc.
-
6th July 2007, 10:56 PM #8Senior Member
- Join Date
- Jul 2007
- Location
- Sydney-south
- Posts
- 333
Cleanliness is next to godliness, use flux if necessary, make sure there is NO water in the pipe at all, dont use the tip of the mapp use the start of the flame and try a stick of 15% silver solder, youll be surprised.
Similar Threads
-
can mapp gas silver solder
By davo_scuba in forum PLUMBING, ELECTRICAL, HEATING, COOLING, etcReplies: 15Last Post: 10th February 2007, 11:28 AM -
How to do reliable silver soldering
By Arron in forum PLUMBING, ELECTRICAL, HEATING, COOLING, etcReplies: 11Last Post: 23rd May 2005, 11:19 AM -
Australian Goverment Pipe Specifications
By trevorZ in forum JOKESReplies: 1Last Post: 28th May 2003, 12:59 AM
Bookmarks