Will Ammonium Persulphate Etch Glass
I've got some for making printed circuits
but wondering if it will etch (corrode) glass
-
1st January 2007, 11:47 AM #2Senior Member
- Join Date
- Jul 2003
- Location
- rural qld
- Age
- 68
- Posts
- 139
just been told that it WONT etch glass and taht its very dangerous stuff as well
-
1st January 2007, 11:56 AM #3
-
1st January 2007, 12:00 PM #4
I've got some and was just wondering if it would.
It doesn't so I'll find something else.
Thank to everyone for your valuable input
-
1st January 2007, 01:39 PM #5
Bob,
AFAIK besides abrasive blasting and other mechanical methods the only thing that will etch glass is Hydrofluoric acid. This is extrmely nasty stuff. We used it in the boat yard to etch the ally before painting and the watered down wash up had to be collected in a tank full of marble chips before it could go into the drains. I don't know what strength is required for glass etching but I do know that the Ali-brite we used would mark windows. When I was looking at the OH&S stuff I read about a pool technician who spilt some concentrate on himself. He jumped in the pool straight away to try to neutralise it. They had him in hospital and whipped off his leg the same day but he was still dead within a week.
Way back when I was screen printing a bloke I worked for got some specialist ink that had hydrofluoric acid in it as he wanted to print an etched logo onto glass. It may still be available now, but it's much easier to use a vinyl cutter to cut the logo on some "frosted" clear sticker to give the same effect. Otherwise you can get a mask made for your logo by a vinyl cutter, apply it to your glass and sandblast the exposed glass lightly.
Mick"If you need a machine today and don't buy it,
tomorrow you will have paid for it and not have it."
- Henry Ford 1938
-
1st January 2007, 03:29 PM #6
I have one of those "201 formulas" books somewhere, will have a look for it, I thought it had a chemical recipe for glass etching.
Will have a sniff around.
Cheers..........Sean
The beatings will continue until morale improves.
-
1st January 2007, 03:46 PM #7
Good news - found it straight away.
Bad news - it recommended hydrofluoric acid
Sorry mate.............cheers.............Sean
The beatings will continue until morale improves.
-
1st January 2007, 05:06 PM #8
Thanks for the looking fellas,
I WON"T use hydrofluoric acid. (or even Nitric)
You don't feel it on the skin, just feels like water,
until it sinks deeper and starts eating your bone away - then it hurts.
Similar Threads
-
Low e glass V glass + film
By doug1 in forum DOORS, WINDOWS, ARCHITRAVES & SKIRTS ETCReplies: 10Last Post: 19th December 2006, 10:53 PM -
Saftey Glass for Windows
By Cobber in forum DOORS, WINDOWS, ARCHITRAVES & SKIRTS ETCReplies: 6Last Post: 20th August 2006, 06:23 PM -
glass coating product found!
By Mybrains in forum GENERAL ODDS N SODSReplies: 3Last Post: 27th March 2006, 09:14 PM
Bookmarks